EN8 ELECTRO GALV STUD M12X160 Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched..
R28.35
Ex Tax:R28.35
Brand: ANCHORS DIRE
Model: RSEG12X170EN8
EN8 ELECTRO GALV STUD M12X170 Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched..
R29.40
Ex Tax:R29.40
Brand: ANCHORS DIRE
Model: RSEG16X125EN8
EN8 ELECTRO GALV STUD M16X125 Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched..
R33.60
Ex Tax:R33.60
Brand: ANCHORS DIRE
Model: RSEG16X190EN8
EN8 ELECTRO GALV STUD M16X190 Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched..
R47.25
Ex Tax:R47.25
Brand: ANCHORS DIRE
Model: RSEG16X220EN8
EN8 ELECTRO GALV STUD M16X220Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched ..
R47.80
Ex Tax:R47.80
Brand: ANCHORS DIRE
Model: RSEG20X170EN8
EN8 ELECTRO GALV STUD M20X170Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched ..
R69.30
Ex Tax:R69.30
Brand: ANCHORS DIRE
Model: RSEG20X240EN8
EN8 ELECTRO GALV STUD M20X240Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched ..
R92.40
Ex Tax:R92.40
Brand: ANCHORS DIRE
Model: RSEG8X130EN8
EN8 ELECTRO GALV STUD M8X130Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched a..
R10.50
Ex Tax:R10.50
Brand: ANCHORS DIRE
Model: RSHDG10X150EN8
EN8 HOT DIP GALV STUD M10X150Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched ..
R21.00
Ex Tax:R21.00
Brand: ANCHORS DIRE
Model: RSHDG10X250EN8
EN8 HOT DIP GALV STUD M10X250Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched ..
R32.55
Ex Tax:R32.55
Brand: ANCHORS DIRE
Model: RSHDG10X90EN8
EN8 HOT DIP GALV STUD M10X90Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched a..
R13.65
Ex Tax:R13.65
Brand: ANCHORS DIRE
Model: RSHDG12X110EN8
EN8 HOT DIP GALV STUD M12X110 Explaining the difference between EN8 and 8.8 steel as indicted8.8 is ISO 898–1 grading for Bolts and screws. It indicates a bolt/screw withtensile strength of minimum 800MPa and a yield strength of 80% of 800MPa = 640MPa.Depending on thickness these are either quenched..
R24.15
Ex Tax:R24.15